Overspray
Definition
Finely atomized paint droplets from the painting process stuck to the surface, or paint droplets that have not been absorbed by the paint film.
![Spritznebel](https://www.glasurit.com/sites/glasurit.com/files/styles/image_medium/public/s.-34.jpg?itok=2vFA8fNg)
Causes
- Poor overspray absorption due to wrong choice of hardener and/or reducer for the ambient painting conditions
- Insufficient masking of adjacent panels/surfaces
![Spritznebel](https://www.glasurit.com/sites/glasurit.com/files/styles/image_medium/public/s_49.jpg?itok=4pg44_R7)
200 x magnification
- Select hardener and reducer that suit the temperature of the workshop and the size of the object/vehicle to be painted (see temperature table).
- Mask panels/surfaces that will not be painted.
- Recommendation for overall resprays: Harmonize overlapping area with Glasurit 352-500 Spot Blender.
REPAIR
Polish with Glasurit 562-1602 Fine Polishing Compound and finish with any standard high-gloss polish.